{"id":1411,"date":"2025-12-25T03:11:40","date_gmt":"2025-12-25T03:11:40","guid":{"rendered":"https:\/\/bomissteel.com\/?p=1411"},"modified":"2026-06-08T09:18:57","modified_gmt":"2026-06-08T01:18:57","slug":"ppgi-vs-ppgl-differences-buying-guide","status":"publish","type":"post","link":"https:\/\/www.bomissteel.com\/az\/ppgi-vs-ppgl-differences-buying-guide\/","title":{"rendered":"PPGI v\u0259 PPGL: Sat\u0131n almadan \u0259vv\u0259l bilm\u0259li oldu\u011funuz 5 \u0259sas f\u0259rq (2026-c\u0131 il \u00fc\u00e7\u00fcn t\u0259limat)"},"content":{"rendered":"<p>\u018fvv\u0259lc\u0259d\u0259n r\u0259ngl\u0259nmi\u015f sinkl\u0259nmi\u015f polad (PPGI) v\u0259 \u0259vv\u0259lc\u0259d\u0259n r\u0259ngl\u0259nmi\u015f qalvalum polad (PPGL) metal konstruksiyalar \u00fc\u00e7\u00fcn \u0259n \u00e7ox istifad\u0259 edil\u0259n materiald\u0131r v\u0259 buna g\u00f6r\u0259 d\u0259 m\u0259\u015fhur metal tikinti material\u0131d\u0131r. Buna g\u00f6r\u0259 d\u0259, h\u0259r ikisini qiym\u0259tl\u0259ndir\u0259rk\u0259n, iki m\u0259hlulun f\u0259rqli \u00fcst\u00fcnl\u00fckl\u0259rini v\u0259 m\u0259nfi c\u0259h\u0259tl\u0259rini qiym\u0259tl\u0259ndirm\u0259k vacibdir. PPGL v\u0259 PPGI ox\u015far g\u00f6r\u00fcns\u0259 d\u0259, f\u0259rqli m\u00fchitl\u0259rd\u0259 istifad\u0259 \u00fc\u00e7\u00fcn uy\u011fundur.<\/p>\n<p>Both materials start from <a href=\"https:\/\/www.bomissteel.com\/az\/collections\/galvalume-steel-coil\/\">galvalume coils<\/a> or galvanized coils as the base substrate before the paint system is applied. The coil quality directly determines the finished product performance.<\/p>\n<table data-path-to-node=\"16\">\n<thead>\n<tr>\n<td><strong>X\u00fcsusiyy\u0259t<\/strong><\/td>\n<td><strong><a class=\"wpil_keyword_link\" href=\"https:\/\/www.bomissteel.com\/az\/collections\/ppgi-coil\/\"   title=\"PPGI\" data-wpil-keyword-link=\"linked\"  data-wpil-monitor-id=\"374\">PPGI<\/a> (Sinkl\u0259nmi\u015f)<\/strong><\/td>\n<td><strong><a class=\"wpil_keyword_link\" href=\"https:\/\/www.bomissteel.com\/az\/collections\/ppgl-coil\/\"   title=\"PPGL\" data-wpil-keyword-link=\"linked\"  data-wpil-monitor-id=\"297\">PPGL<\/a> (Galvalume)<\/strong><\/td>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td><span data-path-to-node=\"16,1,0,0\"><b data-path-to-node=\"16,1,0,0\" data-index-in-node=\"0\">\u00d6rt\u00fck<\/b><\/span><\/td>\n<td><span data-path-to-node=\"16,1,1,0\">100% Sink<\/span><\/td>\n<td><span data-path-to-node=\"16,1,2,0\">55% Al, 43.4% Zn, 1.6% Si<\/span><\/td>\n<\/tr>\n<tr>\n<td><span data-path-to-node=\"16,2,0,0\"><b data-path-to-node=\"16,2,0,0\" data-index-in-node=\"0\">Davaml\u0131l\u0131q<\/b><\/span><\/td>\n<td><span data-path-to-node=\"16,2,1,0\">Standart (10-15 il)<\/span><\/td>\n<td><span data-path-to-node=\"16,2,2,0\">\u00dcst\u00fcn (20-40 ya\u015f)<\/span><\/td>\n<\/tr>\n<tr>\n<td><span data-path-to-node=\"16,3,0,0\"><b data-path-to-node=\"16,3,0,0\" data-index-in-node=\"0\">\u0130stilik M\u00fcqavim\u0259ti<\/b><\/span><\/td>\n<td><span data-path-to-node=\"16,3,1,0\">200\u00b0C-y\u0259 q\u0259d\u0259r<\/span><\/td>\n<td><span data-path-to-node=\"16,3,2,0\">315\u00b0C-y\u0259 q\u0259d\u0259r<\/span><\/td>\n<\/tr>\n<tr>\n<td><span data-path-to-node=\"16,4,0,0\"><b data-path-to-node=\"16,4,0,0\" data-index-in-node=\"0\">\u018fn Yax\u015f\u0131s\u0131<\/b><\/span><\/td>\n<td><span data-path-to-node=\"16,4,1,0\">\u015e\u0259h\u0259r\/S\u0259naye<\/span><\/td>\n<td><span data-path-to-node=\"16,4,2,0\">Sahil\/Y\u00fcks\u0259k \u0130stilikli B\u00f6lg\u0259l\u0259r<\/span><\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<h3>PPGL n\u0259dir? PPGI n\u0259dir?<\/h3>\n<p>PPGI, sink t\u0259b\u0259q\u0259sinin \u00fcz s\u0259thin\u0259 \u00f6rt\u00fck kimi t\u0259tbiq edilm\u0259si v\u0259 keyfiyy\u0259tli boya \u00f6rt\u00fcy\u00fc daxil olmaqla sinkl\u0259m\u0259 m\u0259rh\u0259l\u0259si il\u0259 haz\u0131rlan\u0131r. Bu sink \u00f6rt\u00fcy\u00fc polad\u0131 pasdan qoruyan \u0259la korroziyaya davaml\u0131l\u0131\u011fa malikdir. Boyal\u0131 s\u0259th yaln\u0131z yax\u015f\u0131 g\u00f6r\u00fcnm\u00fcr, h\u0259m d\u0259 ultrab\u0259n\u00f6v\u015f\u0259yi \u015f\u00fcalar, ya\u011f\u0131\u015f, ya\u011f\u0131\u015fl\u0131 hava v\u0259 kimy\u0259vi madd\u0259l\u0259r kimi \u0259traf m\u00fchitin z\u0259r\u0259rli t\u0259sirl\u0259rin\u0259 qar\u015f\u0131 \u0259lav\u0259 bir m\u00fcdafi\u0259 x\u0259ttidir.<br \/>\nPPGL: \u018fvv\u0259lc\u0259d\u0259n r\u0259ngl\u0259nmi\u015f formada qalvalume polad. M\u00fcqayis\u0259 \u00fc\u00e7\u00fcn, PPGL-in \u00f6rt\u00fcy\u00fc al\u00fcminium, sink v\u0259 az miqdarda silikondan ibar\u0259tdir. Bu patentl\u0259\u015fdirilmi\u015f \u0259rinti \u00f6rt\u00fcy\u00fc olan Galvalume, \u0259n\u0259n\u0259vi sinkl\u0259nmi\u015f \u00f6rt\u00fcy\u0259 nisb\u0259t\u0259n daha y\u00fcks\u0259k korroziyaya davaml\u0131l\u0131q t\u0259min edir. M\u0259s\u0259l\u0259n, \u00f6rt\u00fcy\u0259 daxil edilmi\u015f al\u00fcminium g\u0259l\u0259c\u0259k korroziyadan qoruyacaq qal\u0131n bir qoruyucu oksid t\u0259b\u0259q\u0259si yarad\u0131r v\u0259 sink oksid t\u0259b\u0259q\u0259si z\u0259d\u0259l\u0259ndiyi t\u0259qdird\u0259 qurbanl\u0131q qoruma t\u0259min edir. PPGI kimi, PPGL d\u0259 g\u00f6r\u00fcn\u00fc\u015f\u00fcn\u00fc art\u0131rmaq v\u0259 \u0259lav\u0259 qoruma t\u0259klif etm\u0259k \u00fc\u00e7\u00fcn r\u0259ngl\u0259nir. Se\u00e7\u0259rk\u0259n diqq\u0259t yetirilm\u0259li m\u0259qamlar:<\/p>\n<p><img fetchpriority=\"high\" decoding=\"async\" class=\"wp-image-1412 aligncenter\" src=\"https:\/\/bomissteel.com\/wp-content\/uploads\/2025\/12\/\u751f\u6210-PPGL-\u6d82\u5c42\u5c55\u793a\u56fe-scaled.png\" alt=\"PPGL\" width=\"790\" height=\"444\" srcset=\"https:\/\/www.bomissteel.com\/wp-content\/uploads\/2025\/12\/\u751f\u6210-PPGL-\u6d82\u5c42\u5c55\u793a\u56fe-scaled.png 2560w, https:\/\/www.bomissteel.com\/wp-content\/uploads\/2025\/12\/\u751f\u6210-PPGL-\u6d82\u5c42\u5c55\u793a\u56fe-300x169.png 300w, https:\/\/www.bomissteel.com\/wp-content\/uploads\/2025\/12\/\u751f\u6210-PPGL-\u6d82\u5c42\u5c55\u793a\u56fe-1024x576.png 1024w, https:\/\/www.bomissteel.com\/wp-content\/uploads\/2025\/12\/\u751f\u6210-PPGL-\u6d82\u5c42\u5c55\u793a\u56fe-768x432.png 768w, https:\/\/www.bomissteel.com\/wp-content\/uploads\/2025\/12\/\u751f\u6210-PPGL-\u6d82\u5c42\u5c55\u793a\u56fe-1536x864.png 1536w, https:\/\/www.bomissteel.com\/wp-content\/uploads\/2025\/12\/\u751f\u6210-PPGL-\u6d82\u5c42\u5c55\u793a\u56fe-2048x1152.png 2048w, https:\/\/www.bomissteel.com\/wp-content\/uploads\/2025\/12\/\u751f\u6210-PPGL-\u6d82\u5c42\u5c55\u793a\u56fe-600x337.png 600w\" sizes=\"(max-width: 790px) 100vw, 790px\" \/><\/p>\n<h3>Korroziyaya davaml\u0131l\u0131q.<\/h3>\n<p>PPGI v\u0259 PPGL-i m\u00fcqayis\u0259 ed\u0259rk\u0259n, korroziyaya davaml\u0131l\u0131q \u0259sas amill\u0259rd\u0259n biridir. PPGL ya\u015f, duzlu sprey v\u0259 ya korroziyal\u0131 m\u00fchitl\u0259r\u0259 yerl\u0259\u015fdirildikd\u0259 v\u0259 ya t\u0259tbiq edildikd\u0259 v\u0259 ya kimy\u0259vi madd\u0259l\u0259rin i\u015ftirak\u0131 il\u0259 \u00fcst\u00fcnl\u00fcy\u0259 malikdir. PPGL h\u0259m sahil, h\u0259m d\u0259 s\u0259naye b\u00f6lg\u0259l\u0259rind\u0259, s\u0259naye sah\u0259l\u0259rind\u0259 v\u0259 a\u011f\u0131r s\u0259naye i\u015fl\u0259rind\u0259 a\u011f\u0131r t\u0259tbiql\u0259r \u00fc\u00e7\u00fcn yarad\u0131lm\u0131\u015fd\u0131r.<br \/>\nm\u00fchitl\u0259rd\u0259, y\u00fcks\u0259k korroziyaya davaml\u0131l\u0131q \u00fc\u00e7\u00fcn al\u00fcminium-sink \u00f6rt\u00fcy\u00fcn\u00fcn \u00fcst\u00fcnl\u00fcy\u00fc \u0259la korroziyaya davaml\u0131l\u0131qd\u0131r. PPGI h\u0259m\u00e7inin \u0259la korroziyaya davaml\u0131l\u0131\u011fa malikdir, lakin yen\u0259 d\u0259 \u0259la korroziyaya davaml\u0131l\u0131\u011fa baxmayaraq, h\u0259ddind\u0259n art\u0131q korroziya \u00fc\u00e7\u00fcn PPGL performans\u0131ndan bir q\u0259d\u0259r a\u015fa\u011f\u0131 ola bil\u0259r.<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"wp-image-1413 aligncenter\" src=\"https:\/\/bomissteel.com\/wp-content\/uploads\/2025\/12\/Main-03-3.jpg\" alt=\"PPGL\" width=\"600\" height=\"600\" srcset=\"https:\/\/www.bomissteel.com\/wp-content\/uploads\/2025\/12\/Main-03-3.jpg 750w, https:\/\/www.bomissteel.com\/wp-content\/uploads\/2025\/12\/Main-03-3-300x300.jpg 300w, https:\/\/www.bomissteel.com\/wp-content\/uploads\/2025\/12\/Main-03-3-150x150.jpg 150w, https:\/\/www.bomissteel.com\/wp-content\/uploads\/2025\/12\/Main-03-3-500x500.jpg 500w, https:\/\/www.bomissteel.com\/wp-content\/uploads\/2025\/12\/Main-03-3-600x600.jpg 600w, https:\/\/www.bomissteel.com\/wp-content\/uploads\/2025\/12\/Main-03-3-100x100.jpg 100w\" sizes=\"auto, (max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>X\u0259rc-s\u0259m\u0259r\u0259lilik. Tikinti\/istehsal layih\u0259l\u0259ri h\u0259mi\u015f\u0259 maya d\u0259y\u0259rin\u0259 meyllidir. \u018fslind\u0259, PPGI, iki \u00f6rt\u00fck n\u00f6v\u00fc aras\u0131ndak\u0131 f\u0259rq\u0259 g\u00f6r\u0259, ad\u0259t\u0259n toplu olaraq PPGL-d\u0259n daha ucuzdur. Sinkl\u0259nmi\u015f d\u0259mir daha sad\u0259 v\u0259 daha \u0259lveri\u015fli bir materiald\u0131r v\u0259 buna g\u00f6r\u0259 d\u0259 onu daha ucuz edir. \u018fg\u0259r b\u00fcdc\u0259niz m\u0259hduddursa v\u0259 \u0259n yax\u015f\u0131 pas m\u00fcqavim\u0259tini axtarm\u0131rs\u0131n\u0131zsa, PPGI daha s\u0259m\u0259r\u0259li olma ehtimal\u0131 var. M\u0259hsulun uzunm\u00fcdd\u0259tli saxlanmas\u0131 v\u0259 d\u0259yi\u015fdirilm\u0259si x\u0259rcl\u0259rini n\u0259z\u0259r\u0259 alark\u0259n, onu hesablama\u011fa haz\u0131r olmal\u0131y\u0131q, buna g\u00f6r\u0259 d\u0259 \u0259n yax\u015f\u0131 PPGL-in korroziyaya davaml\u0131l\u0131\u011f\u0131n\u0131 n\u0259z\u0259r\u0259 almaq, \u00f6mr\u00fc boyu \u00fcmumi d\u0259y\u0259ri azald\u0131r. Formala\u015fma v\u0259 \u0130\u015fl\u0259m\u0259 qabiliyy\u0259ti. X\u00fcsusil\u0259 layih\u0259 \u0259yilm\u0259 v\u0259 ya m\u00fcr\u0259kk\u0259b formalar \u00fc\u00e7\u00fcn olduqda, metal\u0131n formala\u015fma v\u0259 i\u015fl\u0259m\u0259 qabiliyy\u0259ti d\u0259 vacibdir. PPGI (v\u0259 ya PPGL) d\u0259 haz\u0131rlamaq v\u0259 emal etm\u0259k asand\u0131r, baxmayaraq ki, xarakterik \u00f6rt\u00fcy\u00fcn\u0259 g\u00f6r\u0259 PPGL-in ki\u00e7ik bir formala\u015fma \u00fcst\u00fcnl\u00fcy\u00fc var. Materiallarda istifad\u0259 edildikd\u0259, Galvalume \u00f6rt\u00fckl\u00fc sah\u0259d\u0259 m\u00f6vcud olan al\u00fcminium \u00fcst\u00fcnl\u00fckd\u00fcr, \u00e7\u00fcnki \u00e7atlama v\u0259 ya soyulma \u0259v\u0259zin\u0259 \u0259yilm\u0259 zaman\u0131 elastikliyin artmas\u0131na s\u0259b\u0259b oldu\u011fu bilinir. Layih\u0259nizd\u0259 formala\u015fd\u0131rma \u00e7ox \u015fey t\u0259l\u0259b edirs\u0259, b\u0259lk\u0259 d\u0259 PPGL cavabd\u0131r.<\/p>\n<h3>T\u0259tbiq Sah\u0259l\u0259ri:<\/h3>\n<p>PPGI v\u0259 PPGL Layih\u0259 t\u0259tbiq sah\u0259nizin m\u0259nas\u0131 odur ki, PPGI v\u0259 ya PPGL istifad\u0259 etm\u0259yinizi m\u00fc\u0259yy\u0259n ed\u0259c\u0259k \u0259n g\u00fccl\u00fc amil bu olacaq. Bu, PPGI v\u0259 ya PPGL t\u0259tbiq sah\u0259sidir, \u00e7\u00fcnki PPGI layih\u0259nizin formala\u015fmas\u0131 g\u00f6zl\u0259nil\u0259n sah\u0259dir. PPGI, orta korroziyaya davaml\u0131l\u0131\u011f\u0131n kifay\u0259t q\u0259d\u0259r oldu\u011fu dam \u00f6rt\u00fcy\u00fc, divar \u00f6rt\u00fcy\u00fc v\u0259 adi binalar kimi yerl\u0259rd\u0259 geni\u015f istifad\u0259 olunur. Bundan \u0259lav\u0259, ucuz v\u0259 istifad\u0259si asand\u0131r; bu, onun DIY tikinti material\u0131 kimi populyarl\u0131\u011f\u0131n\u0131 izah edir. PPGL, x\u00fcsusil\u0259 d\u0259niz suyu, kimy\u0259vi madd\u0259l\u0259r v\u0259 enerji daxil olmaqla y\u00fcks\u0259k korroziyaya davaml\u0131 t\u0259tbiql\u0259r, d\u0259niz v\u0259 sahil binalar\u0131 v\u0259 elektrik stansiyalar\u0131 t\u0259tbiql\u0259ri \u00fc\u00e7\u00fcn uy\u011fundur. V\u0259 daha y\u00fcks\u0259k davaml\u0131l\u0131\u011f\u0131 v\u0259 g\u00f6r\u00fcn\u00fc\u015f\u00fcn\u0259 g\u00f6r\u0259 avtomobil v\u0259 m\u0259i\u015f\u0259t texnikas\u0131 s\u0259nayesind\u0259 istifad\u0259 olunur.<\/p>","protected":false},"excerpt":{"rendered":"<p>Pre-painted galvanized steel (PPGI) and pre-painted galvalume steel (PPGL) are the most commonly used material for metal construction and are therefore a popular metal building material. Therefore, in weighing the two, it is important to weigh the distinct virtues and the vices of the 2 solutions. Although PPGL and PPGI might seem to be similar, [&hellip;]<\/p>\n","protected":false},"author":1,"featured_media":1414,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"footnotes":"","rank_math_title":"PPGI vs. PPGL: 5 Key Differences You Must Know (2026 Guide)","rank_math_description":"Confused between PPGI and PPGL? Discover the 5 critical differences in coating composition, corrosion resistance, and lifespan. Our 2026 expert guide helps you choose the most cost-effective color coated steel for your specific environment. Read before you buy!","rank_math_canonical_url":"","rank_math_focus_keyword":""},"categories":[11],"tags":[],"class_list":["post-1411","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-blog"],"_links":{"self":[{"href":"https:\/\/www.bomissteel.com\/az\/wp-json\/wp\/v2\/posts\/1411","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/www.bomissteel.com\/az\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/www.bomissteel.com\/az\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/www.bomissteel.com\/az\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/www.bomissteel.com\/az\/wp-json\/wp\/v2\/comments?post=1411"}],"version-history":[{"count":11,"href":"https:\/\/www.bomissteel.com\/az\/wp-json\/wp\/v2\/posts\/1411\/revisions"}],"predecessor-version":[{"id":7225,"href":"https:\/\/www.bomissteel.com\/az\/wp-json\/wp\/v2\/posts\/1411\/revisions\/7225"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/www.bomissteel.com\/az\/wp-json\/wp\/v2\/media\/1414"}],"wp:attachment":[{"href":"https:\/\/www.bomissteel.com\/az\/wp-json\/wp\/v2\/media?parent=1411"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/www.bomissteel.com\/az\/wp-json\/wp\/v2\/categories?post=1411"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/www.bomissteel.com\/az\/wp-json\/wp\/v2\/tags?post=1411"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}